A fully automated analyzer for surface area and pore size measurements.
-
Offers simultaneous analysis and sample preparation.
-
Low maintenance, vacuum volumetric system with stainless steel manifold construction.
-
Speed and precision ensured by MaxiDose, a proprietary dosing algorithm.
-
High sensitivity ensured by multiple pressure transducers, minimum void volume and accurate coolant level control.
-
Operates with any non-corrosive adsorbate and a wide variety of coolants, including slurries.
-
DoseWizard learn mode and InitialFill for analysis time savings of up to 60 percent.
-
System supplied complete and ready for operation.